PTM-80 CNC/Machine Torch 25FT
CNC / Machine Plasma Torches
SKU# EV-PTM80
80 Amps CNC/Machine Blowback Start version of IPT-80 Plasma Torch Straight head Back Striking design starts arc on shoulder Innotech PTM-80 Central Connector Handle length: 1 ft. (12 inch) Handle diameter: 34.5 mm (1.360 inch) Cable: 25 ft. Made in Italy Fits the following units: PowerPlasma 82i Recommended for older models: PowerPlasma 80S