SKU# PIT-200T
IGBT Type: | Individual IGBT |
Inverter Type: | Digital/Micro-controlled |
Output Type: | D D |
Voltage/phase: | DUAL VOLTAGE 120/240 1 PHASE |
Max Rated TIG Amps: | 200 |
Max Rated Stick Amps: | 160 |
TIG Amps @ Rated Duty Cycle: | 1 2 |
Stick Amps @ Rated Duty Cycle: | 1 2 |
Max Inrush ( I1MAX ) Amps: | 1 2 |
Maximum Rated (I1EFF ) Input Amps: | 1 2 |
OCV: | T S |
TIG Output Range DC: | 3A-200A/10.2V-18V |
Stick Ouput Range DC: | 5A- 160A/20.2V-26.4V |
Stick Hot Start Amps: | 0-100% |
Stick Function: | Adjustable Arc Force Control |
Stick Hot Start Type: | Adjustable Hot Start |
Stick Hot Start Time: | 0-2.5 Seconds |
6010/Cellulose Capable: | Limited to 6011 |
Minimum Amp DC TIG Start: | 3A |
TIG Start Type: | H L |
Memory: | Yes |
Start Amp Range: | 5A-200A |
End Amp Range: | 3A-200A |
Upslope Time: | 0-25 Seconds |
Down Slope Time: | 0-25 Seconds |
Preflow time: | 0-25 Seconds |
Post Flow Time: | 0-25 Seconds |
TIG Pulse: | Yes |
Standard DC Pulse Frequency: | .1-500Hz |
Pulse Time On (Duty Cycle): | 5-100% |
Pulse Amp Range: | 5-95% |
Remote Control: | 2T/4T |
Foot Pedal: | Optional |