$0.00
Go to Checkout
WARNING! Cancer and Reproductive Harm www.p65warnings.ca.gov
SKU# EV-GM0502-BSL-15

Blue Steel Liner .023"-.035" 15FT / 5m

Steel Liners (Hard & Flux Core Wires)
$18.00
Product Overview
Blue Steel Liner .023"-.035" 15FT / 5m
Steel Liners (Hard & Flux Core Wires)

SKU# EV-GM0502-BSL-15

Blue Liner for steel (hard) wire Coated steel 15 ft. / 5m long Fits wire 0.6mm-0.9mm / .023"-.035" Interchanges with Trafimet® GM0502 Interchanges with Binzel® 124.0011 P/N: IIC0507